TEST TEST METHOD TYPICAL VALUES UNIT
Density DIN 53479 A 1.19 g/cm³
Hardness DIN 53505 60 Shore A
Tensile Strength DIN 53504 (S1) 12 N/mm²
Elongation to break DIN 53504 (S1) 600 %
Tear Strength DIN 53515 (C1) 18 N/mm
Compression Set DIN 53517 11 %
Temperature Range -60°C to + 200°C (Continuous)
+260°C (Intermittent)
Dissipation Factor VDE 0303 70 x 10¯⁴ Tan Ō
Dielectric Strength VDE 0303 19 Kv/MM
Dielectric Constant DIN 53482 3 N/A
@ 25°C and 50Hz
Arc Resistance VDE 0441 90 seconds
Surface Resistance VDE 0303 5x 10¹² Ω.cm
Volume Resistivity VDE 0303 5×10¹⁵ Ω.cm
Abrasion Resisitance DIN 53516 76 mm³
Thermal Conductivity DIN 52612 0.25 W·m¯¹·K¯¹
Coefficient of Expansion DIN 52612 3 x 10¯⁴ K¯¹
Weathering DIN 50018 -SFW 2.0 S Without changes 15 cycles
Flame Retardancy UL 94 V 1 pass
Oil Resistance Hardness Change -2 %
ASTM Oil Tensile Strength -10 %
Elongation Change 5 %
Volume Chance 3.8 %